Related Experiment Video
Updated: Aug 28, 2025

A Standard and Reliable Method to Fabricate Two-Dimensional Nanoelectronics
Published on: August 28, 2018
Bottom-up plasma-enhanced atomic layer deposition of SiO2 by utilizing growth inhibition using NH3 plasma
Yoenju Choi1,2, Taehoon Kim2, Hangyul Lee2
1Department of Advanced Materials Engineering for Information and Electronics, and Integrated Education Program for Frontier Science and Technology (BK21 Four), Kyung Hee University, Yongin, Gyeonggi, 17104, Korea.
Abstract:
The design-rule shrinkage in semiconductor devices is a challenge at every step of the integration process. In the gap-fill process for isolation, the seam and void formation cannot be suppressed by using a deposition process, which even has excellent step coverage. To achieve seamless gap fill in the high-aspect-ratio structure, which has a non-ideal etch profile such as a negative slope, the deposition process should be able to realize the "bottom-up growth" behavior. In this work, the bottom-up growth of a SiO2 plasma-enhanced atomic layer deposition (PE-ALD) process in a trench structure was investigated by using a growth inhibition process employing plasma treatment. N2 and NH3 plasma pre-treatments were employed to suppress the growth of the SiO2 PE-ALD process without any contamination, and the inhibition mechanism was investigated by performing surface chemistry analyses using X-ray photoelectron spectroscopy. Furthermore, the gap-fill characteristics of the SiO2 PE-ALD process were examined, depending on the process conditions of NH3 plasma pre-treatment, by performing cross-sectional field emission scanning electron microscopy measurements. Finally, a seamless gap-fill process in a high-aspect-ratio trench pattern was achieved by the bottom-up growth behavior of SiO2 PE-ALD using NH3 plasma pre-treatment.