Abstract:
The mechanical properties of cementitious composites before and after exposure to high temperature are affected by calcium-silicate-hydrate (C-S-H) gels. To evaluate the effects of high temperature, plyvinyl alcohol (PVA) fiber content, and the cooling method on properties of cementitious composites, physical, mechanical, and microscopic tests were performed in this study. The target temperatures were 25, 100, 200, 300, 400, 600, and 800 °C. The PVA fiber contents were 0.0, 0.3, 0.6, 0.9, 1.2, and 1.5 vol%. The high-temperature resistance of PVA fiber-reinforced cementitious composite (PVA-FRCC) specimens was investigated through changes in their appearance, mass loss, compressive strength, splitting tensile strength, flexural strength, and microstructure. The results showed that PVA fibers reduced the probability of explosion spalling in the PVA-FRCC specimens exposed to high temperatures. The mass loss rate of samples exposed to temperatures below 200 °C was small and lower than 5%, whereas a significant mass loss was observed at 200 °C to 800 °C. A small rise in the cubic compressive and splitting tensile strengths of samples was found at 400 °C and 300 °C, respectively. Below 400 °C, the fibers were beneficial to the mechanical strength of the PVA-FRCC specimens. Nevertheless, when the temperature was heated above 400 °C, melted fibers created many pores and channels, which caused a decrease in the strength of the specimens. The method of cooling with water could aggravate the damage to the cementitious composites exposed to temperatures above 200 °C. High temperature could lead to the decomposition of the C-S-H gels of the PVA-FRCC samples, which makes C-S-H gels lose their bonding ability. From the perspective of the microstructure, the structure of PVA-FRCC samples exposed to 600 °C and 800 °C became loose and the number of microcracks increased, which confirmed the reduction in macro-mechanical properties.
More Related Videos
07:15A Testing Platform for Durability Studies of Polymers and Fiber-reinforced Polymer Composites under Concurrent Hygrothermo-mechanical Stimuli
Published on: December 11, 2014
07:48Artificial Thermal Ageing of Polyester Reinforced and Polyvinyl Chloride Coated Technical Fabric
Published on: January 29, 2020
Related Concept Videos
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
Fiber Reinforced Concrete
Strength and Heat of Hydration
The heat of hydration for each cement compound is significant; for instance, tricalcium aluminate (C3A) and...
Abrasion Resistance of Concrete
One such test is the revolving disc test, where three plates...
Types of Cement I
Type I (Ordinary Portland Cement) is widely used for general construction where special properties are not required. It has moderate sulfate resistance and heat of hydration.
Type II (Modified Cement) offers moderate resistance to sulfate attack and a lower rate of heat development compared to Type I. It is suitable for structures in...
Accelerated Curing of Concrete