Characterization of Polyurethane Shape Memory Polymer and Determination of Shape Fixity and Shape Recovery in
Maria Staszczak1, Mana Nabavian Kalat1, Karol Marek Golasiński1
1Institute of Fundamental Technological Research, Polish Academy of Sciences, 02-106 Warsaw, Poland.
Abstract:
Multifunctional polyurethane shape memory polymers (PU-SMPs) have been of increasing interest in various applications. Here we report structure characterization, detailed methodology, and obtained results on the identification of functional properties of a thermoset PU-SMP (MP4510) with glass transition temperature of 45 °C. The stable, chemically crosslinked network of this thermoset PU-SMP results in excellent shape memory behavior. Moreover, the proximity of the activation temperature range of this smart polymer to room and body temperature enables the PU-SMP to be used in more critical industrial applications, namely fast-response actuators. The thermomechanical behavior of a shape memory polymer determines the engineering applications of the material. Therefore, investigation of the shape memory behavior of this class of commercial PU-SMP is of particular importance. The conducted structural characterization confirms its shape memory properties. The shape fixity and shape recovery properties were determined by a modified experimental approach, considering the polymer's sensitivity to external conditions, i.e., the temperature and humidity variations. Three thermomechanical cycles were considered and the methodology used is described in detail. The obtained shape fixity ratio of the PU-SMP was approximately 98% and did not change significantly in the subsequent cycles of the thermomechanical loading due to the stability of chemical crosslinks in the thermoset materials structure. The shape recovery was found to be approximately 90% in the first cycle and reached a value higher than 99% in the third cycle. The results confirm the effect of the thermomechanical training on the improvement of the PU-SMP shape recovery after the first thermomechanical cycle as well as the effect of thermoset material stability on the repeatability of the shape memory parameters quantities.
Related Concept Videos
Plastic Behavior
Polymer Classification: Architecture
Polymer Classification: Stereospecificity
Polymer Classification: Crystallinity
Crystalline domains are the regions where polymer chains are aligned in an orderly manner and held together in proximity by intermolecular forces. For example, chains in the crystalline domains of polyethylene and nylon are bound together by van der Waals...
Plasticity
Molecular Weight of Step-Growth Polymers
As the step-growth polymerization involves step-wise condensation of monomers, the molecular weight also builds up eventually. Consequently, high molecular weight polymers are obtained at the late stages of the polymerization, where 99% of monomers have been consumed.
The extent of the...