Abstract:
Phosphogypsum is an industrial byproduct from the wet preparation of phosphoric acid. Phosphorus building gypsum can be obtained from phosphogypsum after high-thermal dehydration. This study aimed to analyze the influence of ball milling with different parameters on the strength of phosphorus building gypsum. In this paper, the absolute dry flexural strength and the absolute dry compressive strength of phosphorus building gypsum were compared under different mass ratios of material to ball, ball-milling speed, and ball-milling time, and the NSGM (1,4) model was applied to model and predict the strength of phosphorus building gypsum modified by ball milling. According to the research results, under the same mass ratio of material to ball and ball-milling speed, the absolute dry flexural strength and absolute dry compressive strength of phosphorus building gypsum firstly increased and then decreased with the increase in milling time. The NSGM (1,4) model established in this paper could effectively simulate and predict the absolute dry flexural strength and the absolute dry compressive strength of the ball-milling-modified phosphorus building gypsum; the average relative simulation errors were 12.38% and 13.77%, and the average relative prediction errors were 6.30% and 12.47%.
More Related Videos
13:05Reliable Mechanochemistry: Protocols for Reproducible Outcomes of Neat and Liquid Assisted Ball-mill Grinding Experiments
Published on: January 23, 2018
10:36Gelatin Methacryloyl Granular Hydrogel Scaffolds: High-throughput Microgel Fabrication, Lyophilization, Chemical Assembly, and 3D Bioprinting
Published on: December 9, 2022
Related Concept Videos
Mortar Properties
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
Fineness of Cement
Direct...
Types of Cement II