Experimental Static and Dynamic Characteristics of Recycled Waste Tire Rubber Particle-Cement-Sand Composite Soil

Zhaoyan Li1, Liping Zhang2, Haiyang Zhuang1,2

  • 1Institute of Engineering Mechanics, China Earthquake Administration, Harbin 150080, China.

Related Concept Videos

Strength of Cement01:20

Strength of Cement

Strength tests for cement are not performed directly on neat cement paste due to difficulty in obtaining consistent, reliable specimens. Instead, cement is typically tested in the form of cement-sand mortar.
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
194
Abrasion Resistance of Concrete01:23

Abrasion Resistance of Concrete

Abrasion resistance is an essential characteristic of concrete that determines its durability and longevity under various wear conditions. Concrete surfaces are vulnerable to different types of abrasion. For instance, surfaces may wear down due to the constant movement of vehicles or be eroded by solids carried in water, as seen in concrete canal linings. Specific tests are conducted to measure the abrasion resistance of concrete.
One such test is the revolving disc test, where three plates...
177
Fatigue Strength of Concrete01:22

Fatigue Strength of Concrete

Fatigue, in the context of materials science and engineering, refers to the weakening or failure of a material caused by repeatedly applied loads, even if these loads are below the strength limit of the material. Fatigue strength in concrete is a critical property that influences its durability and longevity. Concrete can fail in two ways due to fatigue. Static fatigue or creep rupture occurs under a constant load or one that increases slowly. The other failure mode is due to cyclical or...
245
Behavior of Concrete Under Compressive Load01:23

Behavior of Concrete Under Compressive Load

Concrete exhibits specific behaviors under different compressive loads. Understanding this is crucial for understanding its structural integrity. When concrete undergoes uniaxial compression, it tends to develop cracks that run parallel to the direction of the force. These parallel cracks stem from localized tensile stresses that occur perpendicular to the compression direction. Additionally, angled cracks may appear due to the formation of shear planes.
As the concrete specimen fractures under...
237
Vebe Test01:22

Vebe Test

The Vebe test is a method used to measure the workability of concrete, particularly effective for dry concrete mixes. This test employs a specific apparatus that includes a cylindrical chamber, a standard slump cone, and a transparent disc-shaped rider, all mounted on a vibrating table. The cylindrical chamber has dimensions of nine and a half inches in diameter and eight inches in height.
To conduct the test, concrete is placed into the slump cone. The concrete is filled in layers and...
203
Dynamic Modulus of Elasticity of Concrete01:16

Dynamic Modulus of Elasticity of Concrete

The dynamic modulus of elasticity assesses how a concrete structure deforms under impact or dynamic loads. It is typically higher than the static modulus of elasticity, measured under slow, steady loading conditions.
The sonic test is a common method to determine the dynamic modulus. In this test, a concrete beam, sized either 6 x 6 x 30 inches or 4 x 4 x 20 inches, is clamped at its center. Vibrations are initiated at one end of the beam by an electromagnetic exciter unit powered by...
473