Experimental Characterization of Laser Trepanned Microholes in Superalloy GH4220 with Water-Based Assistance
Liang Wang1, Huayu Yang2, Naifei Ren2
1Faculty of Mechanical and Materials Engineering, Huaiyin Institute of Technology, Huaian 223000, China.
Abstract:
An experiment using water-assisted millisecond laser trepanning on superalloy GH4220 was carried out, and the effects of pulse energy on the hole entrance morphology, diameter, roundness, cross-section morphology, taper angle, sidewall roughness, and recast layer in air and with water-based assistance were compared and analyzed. The results show that, compared with the air condition, the water-based assistance improved the material removal rate and hole quality, increased the diameter of the hole entrance and exit, increased the hole roundness, decreased the hole taper angle, decreased the hole sidewall roughness, and reduced the recast layer thickness. In addition, under the combined action of water and steam inside the hole, the sidewall surface morphology quality was improved. Compared with the air condition, the spatter around the hole entrance was reduced, but the oxidation phenomenon formed by the thermal effect surrounding the hole entrance with water-based assistance was more obvious. The research provided technical support for the industrial application of millisecond laser drilling.
More Related Videos
11:34Subsurface Defect Localization by Structured Heating Using Laser Projected Photothermal Thermography
Published on: May 15, 2017
10:52Conducting Elevated Temperature Normal and Combined Pressure-Shear Plate Impact Experiments Via a Breech-end Sabot Heater System
Published on: August 7, 2018