Carbonated beverages have side effects on oral health and general health. Flexural strength is a prime mechanical property of restorative material. The aim of this study is to know the effect of carbonated beverages on the flexural strength of composite restorative material. Two types of composites (Ivoclar and Restofill) were used as samples for comparative evaluation of flexural strength. The sample size is 10 where 5 of each type of composites are included. The obtained samples were immersed in carbonated beverages. One sample of each type was used as a control. After 24 h, the flexural strength of all the 10 samples was evaluated using the formula (3FL/2bd2), and the values were tabulated. Average values and graphs were done using SPSS software. The results showed the changes in flexural strength of both Ivoclar and Restofill materials when immersed in carbonated beverages. The mean value of all the samples was taken, and the standard deviation was calculated. After immersion in carbonated liquids, the mean value of Ivoclar and Restofill samples is 58.9 and 35.01, respectively. P = 0.718 (>0.05), which was not statistically significant. After immersion in Coke, the Restofill group exhibits more flexural strength than the Ivoclar group composite; however, the strength reduces when immersed in Sprite as compared to the Ivoclar group composite.
Related Concept Videos
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
Carbonation Shrinkage
The concrete's permeability is slightly reduced as calcium carbonate produced during the reaction fills its pores. Furthermore, its strength is slightly enhanced as the water released during the reaction...
Flexural Stress
Hooke's Law states that within the material's elastic limits, stress is directly proportional to strain. In a member experiencing a bending moment, the strain at any point is relative to...
Impact Strength of Concrete
Fiber Reinforced Concrete