Determination of the Dielectric Constant of Niobium Oxide by Using Combined EIS and Ellipsometric Methods
Krzysztof Fitzner1, Michał Stępień1
1Faculty of Non-Ferrous Metals, AGH University of Science and Technology, al. A. Mickiewicza 30, 30-059 Krakow, Poland.
Abstract:
Combining ellipsometric and EIS methods, the dielectric constant ε for the oxide Nb2O5 at room temperature was determined. At first, the linear dependence between anodization voltage and oxide thickness was established in the form d = 2.14 (± 0.05) · U + 12.2 (± 1.7) nm in the range of anodizing potentials 0-50 V. Next, assuming the equivalent circuit corresponds to one, the capacitance C of the dense oxide layer was measured. All results taken together gave the value of dielectric constant ε = 93 ± 5.
Related Concept Videos
Susceptibility, Permittivity and Dielectric Constant
Electrostatic Boundary Conditions in Dielectrics
Consider a case where both the mediums across a boundary are two different dielectric materials. Recall that the electric field and electric displacement are proportional and related through the material's...
Dielectric Polarization in a Capacitor