Ultra-thin ZrO2overcoating on CuO-ZnO-Al2O3catalyst by atomic layer deposition for improved catalytic performance of CO2hydrogenation to dimethyl ether
Xiao Fan1, Baitang Jin1, Xiaoqing He2,3
1Linda and Bipin Doshi Department of Chemical and Biochemical Engineering, Missouri University of Science and Technology, Rolla, MO 65409, United States of America.
Abstract:
An ultra-thin overcoating of zirconium oxide (ZrO2) film on CuO-ZnO-Al2O3(CZA) catalysts by atomic layer deposition (ALD) was proved to enhance the catalytic performance of CZA/HZSM-5 (H form of Zeolite Socony Mobil-5) bifunctional catalysts for hydrogenation of CO2to dimethyl ether (DME). Under optimal reaction conditions (i.e. 240 °C and 2.8 MPa), the yield of product DME increased from 17.22% for the bare CZA/HZSM-5 catalysts, to 18.40% for the CZA catalyst after 5 cycles of ZrO2ALD with HZSM-5 catalyst. All the catalysts modified by ZrO2ALD displayed significantly improved catalytic stability of hydrogenation of CO2to DME reaction, compared to that of CZA/HZSM-5 bifunctional catalysts. The loss of DME yield in 100 h of reaction was greatly mitigated from 6.20% (loss of absolute value) to 3.01% for the CZA catalyst with 20 cycles of ZrO2ALD overcoating. Characterizations including hydrogen temperature programmed reduction, x-ray powder diffraction, and x-ray photoelectron spectroscopy revealed that there was strong interaction between Cu active centers and ZrO2.
Related Concept Videos
Reduction of Alkenes: Catalytic Hydrogenation
Metals like palladium, platinum, and nickel are commonly used in their solid forms — fine powder on an inert surface. As these catalysts remain insoluble in the reaction mixture, they are referred to as heterogeneous catalysts.
The hydrogenation process takes place on the...
Reduction of Alkynes to cis-Alkenes: Catalytic Hydrogenation
Like alkenes, alkynes can be reduced to alkanes in the presence of transition metal catalysts such as Pt, Pd, or Ni. The reaction involves two sequential syn additions of hydrogen via a cis-alkene intermediate.
Reduction of Alkenes: Asymmetric Catalytic Hydrogenation
The metal catalyst used can be either heterogeneous or homogeneous. When hydrogenation of an alkene generates a chiral center, a pair of enantiomeric products is expected to form. However, an enantiomeric excess of one of the products can be facilitated using an enantioselective reaction or an...
Catalysis
Oxidation of Alkenes: Syn Dihydroxylation with Osmium Tetraoxide