Computational Investigation of Precursor Blocking during Area-Selective Atomic Layer Deposition Using Aniline as a

I Tezsevin1, J F W Maas1, M J M Merkx1

  • 1Department of Applied Physics, Eindhoven University of Technology, Post Office Box 513, 5600 MB Eindhoven, Netherlands.

Related Concept Videos

Atomic Absorption Spectroscopy: Interference01:25

Atomic Absorption Spectroscopy: Interference

Interference leads to systematic error in atomic absorption (AA) measurements by enhancing or diminishing the analytical signal or the background. These interferences can be grouped into three main categories: spectral interference, chemical interference, and physical interference.
Spectral interference occurs when signals from other elements or molecules overlap with the analyte signal, falsely elevating or masking the analyte's absorbance. This interference can be corrected using Zeeman,...
889
Preparation of 1° Amines: Azide Synthesis01:22

Preparation of 1° Amines: Azide Synthesis

Direct alkylation of ammonia produces polyalkylated amines, along with a quaternary ammonium salt. To exclusively prepare primary amines, the azide synthesis method can be used.
Azide ions act as good nucleophiles and react with unhindered alkyl halides to form alkyl azides. Alkyl azides do not participate in further nucleophilic substitution reactions, thereby eliminating the chances of polyalkylated products. Alkyl azides are reduced by hydride-based reducing agents, like lithium aluminum...
4.1K
Preparation of Amines: Alkylation of Ammonia and Amines01:30

Preparation of Amines: Alkylation of Ammonia and Amines

Alkylation is one of the methods used to prepare amines. Direct alkylation of ammonia or a primary amine with an alkyl halide gives polyalkylated amines along with a quaternary ammonium salt through successive SN2 reactions. This process of making the quaternary salt through the direct alkylation method is called exhaustive alkylation.
Each alkylation step makes the nitrogen center more nucleophilic, which triggers successive alkylations until a quaternary ammonium salt is formed. Considering...
3.6K
Preparation of 1° Amines: Gabriel Synthesis01:28

Preparation of 1° Amines: Gabriel Synthesis

Direct alkylation is not a suitable method for synthesizing amines because it produces polyalkylated products. Gabriel synthesis is the most preferred method to exclusively make primary amines. The method uses phthalimide, which contains a protected form of nitrogen that participates in alkylation only once to predominantly give primary amines.
Strong bases like NaOH or KOH deprotonate the phthalimide to form the corresponding anion, which acts as a nucleophile. Further, the anion attacks an...
3.7K