Long-chain anionic surfactants enabling stable perovskite/silicon tandems with greatly suppressed stress corrosion

Xinlong Wang1,2, Zhiqin Ying3, Jingming Zheng1

  • 1Ningbo Institute of Materials Technology and Engineering, Chinese Academy of Sciences (CAS), 315201, Ningbo, China.

Nature Communications
|April 15, 2023
PubMed