Long-chain anionic surfactants enabling stable perovskite/silicon tandems with greatly suppressed stress corrosion
Xinlong Wang1,2, Zhiqin Ying3, Jingming Zheng1
1Ningbo Institute of Materials Technology and Engineering, Chinese Academy of Sciences (CAS), 315201, Ningbo, China.
Abstract:
Despite the remarkable rise in the efficiency of perovskite-based solar cells, the stress-induced intrinsic instability of perovskite active layers is widely identified as a critical hurdle for upcoming commercialization. Herein, a long-alkyl-chain anionic surfactant additive is introduced to chemically ameliorate the perovskite crystallization kinetics via surface segregation and micellization, and physically construct a glue-like scaffold to eliminate the residual stresses. As a result, benefiting from the reduced defects, suppressed ion migration and improved energy level alignment, the corresponding unencapsulated perovskite single-junction and perovskite/silicon tandem devices exhibit impressive operational stability with 85.7% and 93.6% of their performance after 3000 h and 450 h at maximum power point tracking under continuous light illumination, providing one of the best stabilities to date under similar test conditions, respectively.
More Related Videos
12:21Preparation of Monodomain Liquid Crystal Elastomers and Liquid Crystal Elastomer Nanocomposites
Published on: February 6, 2016
06:31Studying Surfactant Effects on Hydrate Crystallization at Oil-Water Interfaces Using a Low-Cost Integrated Modular Peltier Device
Published on: March 18, 2020
Related Concept Videos
Surface Active Agents
Micelles