Related Experiment Video
Updated: Aug 2, 2025

Synthesis of Soft Polysiloxane-urea Elastomers for Intraocular Lens Application
Published on: March 8, 2019
Ultrafast synthesis of silicone elastomers using silsesquioxane cages as crosslinkers
Chidchanok Wannasiri1, Supphachok Chanmungkalakul1, Teeraya Bureerug1
1Department of Chemistry, Center of Excellence for Innovation in Chemistry (PERCH-CIC), and Center for Inorganic and Materials Chemistry, Faculty of Science, Mahidol University, Rama VI road, Ratchathewi, Bangkok 10400, Thailand. vuthichai.erv@mahidol.edu.
Abstract:
Cross-linked siloxane/silsesquioxane-based elastomers were easily prepared in 15 min via the anionic ring-opening polymerization of cyclotetrasiloxane (D4) and a polyhedral oligomeric silsesquioxane, using K2CO3 as a catalytic base in dimethylformamide at 70 °C. The resulting silicone elastomers have high mechanical strength, good thermal stability, and good superhydrophobic properties.