Related Experiment Video
Updated: Jul 30, 2025

Fabrication of Mechanically Tunable and Bioactive Metal Scaffolds for Biomedical Applications
Published on: December 8, 2015
Mechanical Energy Absorption Ability of Titanium-Based Porous Structures Produced by Various Powder Metallurgy
Pavlo E Markovsky1,2, Jacek Janiszewski2, Oleksandr O Stasiuk1
1G.V. Kurdyumov Institute for Metal Physics of N.A.S. of Ukraine, 36, Academician Vernadsky Boulevard, 03142 Kyiv, Ukraine.
Abstract:
Porous materials are very efficient in absorbing mechanical energy, for instance, in combined armor, in order to improve the anti-ballistic protection characteristics. In the present study, porous titanium-based structures were manufactured via three different powder metallurgy methods using titanium hydride (TiH2) powder, which provided activated sintering, owing to dehydrogenation. The emission of hydrogen and shrinkage of powder particles on dehydrogenation also added an additional potential to control the sintering process and create desirable porosities. TiH2 powder was sintered with additions of NaCl or ammonium carbide as pore holding removable agents, while highly porous Ti-Al structures were formed via liquid phase reactive sintering of TiH2 and Al powders. The microstructures and porosities of sintered dehydrogenated titanium and Ti-Al structures were comparatively studied. Mechanical characteristics were evaluated using compression testing with strain rates varying from quasi-static to high levels. The resonant frequency method was also employed to determine damping parameters and elastic modulus of these materials. All testing methods were aimed at characterizing the energy-absorbing ability of the obtained porous structures. The desired strength, plasticity and energy-absorbing characteristics of porous titanium-based structures were assessed, and the possibilities of their application were also discussed. Based on the obtained results, it was found that porous titanium materials produced with the use of ammonium carbonate showed promising energy absorption properties.
More Related Videos
06:12Plasma Polishing as a New Polishing Option to Reduce the Surface Roughness of Porous Titanium Alloy for 3D Printing
Published on: April 28, 2023
09:12Production of Single Tracks of Ti-6Al-4V by Directed Energy Deposition to Determine the Layer Thickness for Multilayer Deposition
Published on: March 13, 2018