Introduction:
This study aimed to evaluate the chemomechanical properties and biocompatibility of recently introduced premixed putty-type bioactive ceramic cements (PPBCs).
Methods:
Including ProRoot MTA (PMTA) as a control, BC RRM fast-set putty (BCPT), Well-Root PT (WRPT), One-Fil PT (OFPT), and Endocem MTA premixed (ECPM) were compared to evaluate setting time, radiopacity, pH change, and microhardness. Biocompatibility on human dental pulp cells was compared using CCK-8 assay. Mineralization potential was evaluated using alkaline phosphatase activity, Alizarin Red S (ARS) staining, and quantitative real-time polymerase chain reaction with odontogenic gene marker. For data analysis, 1-way analysis of variance and Tukey's post hoc test were used at the significance level of 95%.
Results:
Among the PPBCs, BCPT presented the longest (552 ± 27) setting time (minutes) and others showed significantly shorter time than PMTA (334 ± 22) (P < .05). WRPT (6.20 ± 0.54) and OFPT (5.82 ± 0.50) showed significantly higher radiopacity values (mmAl) and others showed similar value compared with PMTA (P > .05). All PPBCs showed high alkaline pH from fresh materials and tended to increase according to time periods from 30 minutes to 12 hours. ECPM showed the highest value of microhardness (81.62 ± 5.90), WRPT showed similar, and others showed lower than PMTA (P < .05). All PPBCs showed biocompatibility in CCK-8 assay. All PPBCs showed similar or better value compared with PMTA in ALP and ARS staining, and ALP and DSPP marker expression (P < .05).
Conclusions:
The PPBCs showed clinically acceptable chemomechanical properties and favorable mineralization potential.
More Related Videos
Related Concept Videos
Mortar Properties
Porosity in Cement Paste
The balance of water to cement in the mix is...
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
Soundness of Cement
Mortar
Fineness of Cement
Direct...