A Molecular Dynamics Study on the Dislocation-Precipitate Interaction in a Nickel Based Superalloy during the Tensile

Chang-Feng Wan1, Li-Gang Sun1, Hai-Long Qin2

  • 1School of Science, Harbin Institute of Technology, Shenzhen 518055, China.

PubMed

Related Concept Videos

Stress-Strain Diagram - Ductile Materials01:24

Stress-Strain Diagram - Ductile Materials

The stress-strain relationship in ductile materials such as structural steel or aluminium is intricate and progresses through several stages. When a specimen is loaded, it initially exhibits a linear length increase, depicted by a steep straight line on the stress-strain diagram. It indicates the material is elastically deforming and will return to its original shape once unloaded. However, when a critical stress value is reached, plastic deformation begins. This stage sees substantial...
813
Temperature Dependent Deformation01:12

Temperature Dependent Deformation

In a nonhomogeneous rod made up of steel and brass, restrained at both ends and subjected to a temperature change, several steps are involved in calculating the stress and compressive load. Due to the problem's static indeterminacy, one end support is disconnected, allowing the rod to experience the temperature change freely. Next, an unknown force is applied at the free end, triggering deformations in the rod's steel and brass portions. These deformations are then calculated and added...
161
Precipitation Gravimetry01:03

Precipitation Gravimetry

Precipitation gravimetry is based on converting an analyte into a sparingly soluble precipitate, which is separated by filtration and weighed. An ideal precipitate should be pure, insoluble, of known composition, and easily filtered from the reaction mixture.
In determining nickel by gravimetric analysis, a precipitant of ethanolic dimethylglyoxime is added to a hot nickel salt solution. This is quickly followed by the dropwise addition of dilute ammonia solution until precipitation occurs. A...
6.6K
Plastic Behavior01:21

Plastic Behavior

A material's elastic behavior is characterized by the disappearance of stress once the load is removed, allowing the material to return to its original state. However, when stress surpasses the yield point, yielding commences, marking the onset of plastic deformation or permanent set. This change from elastic to plastic behavior is influenced by the peak stress value and the duration before the load is removed. An intriguing observation occurs when a specimen is loaded, unloaded, and...
218