Flowability and Strength Characteristics of Binary Cementitious Systems Containing Silica Fume, Fly Ash, Metakaolin,
Mohammad Iqbal Khan1, Yassir M Abbas1, Galal Fares1
1Department of Civil Engineering, College of Engineering, King Saud University, P.O. Box 800, Riyadh 11421, Saudi Arabia.
Abstract:
The present study examines the effects of supplementary cementitious materials (SCMs) on the flowability and strength development of binary mixes. This study was primarily motivated by the need to bridge the knowledge gap regarding paste and mortar mixes containing binary cement from a variety of performance perspectives. This study examined the flowability and strength development of binary mixes in their pastes and mortars when they contain various doses of silica fume (SF), fly ash (FA), metakaolin (MK), and glass cullet powder (GP) compared with the control mix. While the presence of SF and MK reduced workability because of the nature of their particles, the addition of FA and GP improved it to a certain extent because of the spherical and glassy nature of their particles, respectively. In addition, GP was used to compare its performance against SF, MK, and FA as an alternative cementitious material. In this study, the GP performed comparably to the other SCMs investigated and was found to be satisfactory. An investigation of the rheological properties, heat of hydration, thermal analysis, and pore systems of these mixes was conducted. Compared to the control mix, the presence of 5% GP improved the rheological properties and reduced the heat of hydration by 10%. The reduced workability in SF and MK mixes resulted in a lower content of pore water, while GP and FA incorporation enhanced it, owing to improved workability. The pore area is related to the pore water, which is directly related to improved workability. According to the following order, SF > MK > GP > FA, the strength was highest for mixes containing SF and MK, whereas, with GP and FA, there was a gradual reduction in the strength proportional to replacement level and improved workability. SF, GP, and FA can be identified as performance enhancers when formulating ternary and quaternary cementitious systems for low-carbon cement.
More Related Videos
06:27Expression of Cementitious Pore Solution and the Analysis of Its Chemical Composition and Resistivity Using X-ray Fluorescence
Published on: September 23, 2018
05:38Production and Analysis of Sporosarcina pasteurii Biocement Bricks Using Custom 3D-Printed Molds for Unconfined Compression Tests
Published on: March 7, 2025
Related Concept Videos
Pozzolans
Fly ash is...
Types of Cement II
Fineness of Cement
Direct...
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...