Related Experiment Video
Updated: Jul 9, 2025

Preparation and Testing of Plant Seed Meal-based Wood Adhesives
Published on: March 5, 2015
Polyurethane Adhesives for Wood Based on a Simple Mixture of Castor Oil and Crude Glycerin
Tábata Larissa Corrêa Peres1, Felipe Vahl Ribeiro2, Arthur Behenck Aramburu3
1Postgraduate Program in Materials Science and Engineering, Federal University of Pelotas, Pelotas 96010-150, RS, Brazil.
Abstract:
Developing a new type of polyurethane is essential because conventional options often exhibit shortcomings in terms of environmental sustainability, cost-effectiveness, and performance in specialized applications. A novel polyurethane adhesive derived from a simple mixture of castor oil (CO) and crude glycerin (CG) holds promise as it reduces reliance on fossil fuels and harnesses renewable resources, making it environmentally friendly. Simple CO/CG mixtures, adjusted at three different weight fractions, were used as bio-based polyester polyols to produce polyurethane adhesive for wood bonding. The resulting products are yellowish liquids with moderate-to-high viscosity, measuring 19,800-21,000 cP at 25 °C. The chemical structure of the polyester polyols was characterized using infrared spectroscopy (FTIR), thermogravimetry (TG), and differential scanning calorimetry (DSC). These polyols reacted with polymeric 4,4-methylene diphenyl diisocyanate (p-MDI) at a consistent isocyanate index of 1.3, resulting in the formation of polyurethane adhesives. Crucially, all final adhesives met the adhesive strength requirements specified by ASTM D-5751 standards, underscoring their suitability for wood bonding applications. The addition of CG enhanced the surface and volumetric hydrophobicity of the cured adhesives, resulting in adhesive properties that are not only stronger but also more weather-resistant. Although the thermal stability of the adhesives decreased with the inclusion of CG, FTIR analysis confirmed proper polyurethane polymer formation. The adhesive adjusted for a 2:1 CO:CG weight ratio promoted wood-wood bonding with the highest shear strength, likely due to a higher formation of urethane linkages between hydroxyl groups from the blend of polyols and isocyanate groups from the p-MDI.
Related Concept Videos
Types of Step-Growth Polymers: Polyesters
Polyesters are commonly prepared from terephthalic acid and ethylene glycol; the crude product is known as poly(ethylene terephthalate) or PET. However, polyesters are synthesized industrially by transesterification of dimethyl terephthalate with ethylene glycol at 150 °C. The two reactants and the...
Wood Products
Glue-laminated wood, often referred to as glulam, combines multiple smaller pieces of dimensional lumber using adhesives to form a single, larger piece. Cross-laminated timber consists...
Wood Panel Products
Wood Surfacing
The equipment used in the surfacing process is a plane equipped with rotating blades. This tool efficiently smoothens the wood surface and can...
Olefin Metathesis Polymerization: Acyclic Diene Metathesis (ADMET)
Similar to cross-metathesis, ADMET also involves the formation of metallacyclobutane intermediate by [2+2] cycloaddition of one of the double bonds of a terminal diene with...
Ethers from Alcohols: Alcohol Dehydration and Williamson Ether Synthesis
Ethers can be prepared from organic compounds by various methods. Some of them are discussed below,
Preparation of Ethers by Alcohol Dehydration
In this method, in the presence of protic acids, alcohol dehydrates to produce alkenes and ethers under different conditions. For example, in the presence of sulphuric acid, dehydration of ethanol at 413 K yields ethoxyethane, whereas it yields ethene at 443 K.