Effect of bio-polyol molecular weight on the structure and properties of polyurethane-polyisocyanurate (PUR-PIR)
Adam Olszewski1,2, Paulina Kosmela3,4, Laima Vēvere5
1Department of Polymer Technology, Chemical Faculty, Gdansk University of Technology, G. Narutowicza St. 11/12, 80-233, Gdansk, Poland. Adam.Olszewski@pg.edu.pl.
Abstract:
The increasing interest in polyurethane materials has raised the question of the environmental impact of these materials. For this reason, the scientists aim to find an extremely difficult balance between new material technologies and sustainable development. This work attempts to validate the possibility of replacing petrochemical polyols with previously synthesized bio-polyols and their impact on the structure and properties of rigid polyurethane-polyisocyanurate (PUR-PIR). To date, biobased polyols were frequently used in the manufacturing of PU, but application of bio-polyols synthesized via solvothermal liquefaction using different chains of polyethylene glycol has not been comprehensively discussed. In this work, ten sets of rigid polyurethane foams were synthesized. The influence of bio-polyols addition on foam properties was investigated by mechanical testing, thermogravimetric analysis (TGA), and cone calorimetry. The structure was determined by scanning electron microscopy (SEM) and a gas pycnometer. The tests revealed a significant extension of foam growth time, which can be explained by possible steric hindrances and the presence of less reactive secondary hydroxyl groups. Moreover, an increase average size of pores and aspect ratio was noticed. This can be interpreted by the modification of the cell growth process by the introduction of a less reactive bio-polyol with different viscosity. The analysis of foams mechanical properties showed that the normalized compressive strength increased up to 40% due to incorporation of more cross-linked structures. The thermogravimetric analysis demonstrated that the addition of bio-based polyols increased temperature of 2% (T2%) and 5% (T5%) mass degradation. On the other hand, evaluation of flammability of manufactured foams showed increase of total heat release (HRR) and smoke release (TSR) what may be caused by reduction of char layer stability. These findings add substantially to our understanding of the incorporation of bio-polyols into industrial polyurethane systems and suggest the necessity of conducting further research on these materials.
More Related Videos
09:09Synthesis of PolyN-isopropylacrylamide Janus Microhydrogels for Anisotropic Thermo-responsiveness and Organophilic/Hydrophilic Loading Capability
Published on: February 27, 2016
15:33Microwave-assisted Functionalization of Polyethylene glycol and On-resin Peptides for Use in Chain Polymerizations and Hydrogel Formation
Published on: October 29, 2013
Related Concept Videos
Molecular Weight of Step-Growth Polymers
As the step-growth polymerization involves step-wise condensation of monomers, the molecular weight also builds up eventually. Consequently, high molecular weight polymers are obtained at the late stages of the polymerization, where 99% of monomers have been consumed.
The extent of the...
Polymers: Molecular Weight Distribution
Polymer Classification: Architecture
Polymers: Defining Molecular Weight
The number average molecular weight (Mn) is the summation of the number...
Polymer Classification: Stereospecificity
Polymer Classification: Crystallinity
Crystalline domains are the regions where polymer chains are aligned in an orderly manner and held together in proximity by intermolecular forces. For example, chains in the crystalline domains of polyethylene and nylon are bound together by van der Waals...