Leveraging Deep Neural Networks for Estimating Vickers Hardness from Nanoindentation Hardness

Junbo Niu1, Bin Miao1, Jiaxu Guo1

  • 1School of Material Science & Engineering, Harbin Institute of Technology, Harbin 150001, China.