The Tunable Rhenium Effect on the Creep Properties of a Nickel-Based Superalloy
1Department of Mechanics, School of Physical Science and Engineering, Beijing Jiaotong University, Beijing 100044, China.
Abstract:
Atomistic simulations on the creep of a nickel-based single-crystal superalloy are performed for examining whether the so-called rhenium effect can be tuned by changing the spatial distribution of rhenium in the nickel matrix phase. Results show that Rhenium dopants at {100} phase interfaces facilitate mobile partial dislocations, which intensify the creep, leading to a larger creep strain than that of a pure Ni/Ni3Al system containing no alloying dopants. If all the Re dopants in the matrix phase are far away from phase interfaces, a conventional retarding effect of Re can be observed. The current study implies a tunable Re effect on creep via dislocation triggering at the phase interfaces.
More Related Videos
11:11Experimental Methods for Investigation of Shape Memory Based Elastocaloric Cooling Processes and Model Validation
Published on: May 2, 2016
14:51An Available Technique for Preparation of New Cast MnCuNiFeZnAl Alloy with Superior Damping Capacity and High Service Temperature
Published on: September 23, 2018
Related Concept Videos
Effects of Creep
Creep in Concrete
Plastic Behavior
Temperature Dependent Deformation