Mechanical Properties of MiniBars™ Basalt Fiber-Reinforced Geopolymer Composites
Gabriel Furtos1, Doina Prodan1, Codruta Sarosi1
1Raluca Ripan Institute of Research in Chemistry, Babes-Bolyai University, 400294 Cluj-Napoca, Romania.
Abstract:
Fly ash-based geopolymers represent a new material, which can be considered an alternative to ordinary Portland cement. MiniBars™ are basalt fiber composites, and they were used to reinforce the geopolymer matrix for the creation of unidirectional MiniBars™ reinforced geopolymer composites (MiniBars™ FRBCs). New materials were obtained by incorporating variable amount of MiniBars™ (0, 12.5, 25, 50, 75 vol.% MiniBars™) in the geopolymer matrix. Geopolymers were prepared by mixing fly ash powder with Na2SiO3 and NaOH as alkaline activators. MiniBars™ FRBCs were cured at 70 °C for 48 h and tested for different mechanical properties. Optical microscopy and SEM were employed to investigate the fillers and MiniBars™ FRBC. MiniBars™ FRBC showed increasing mechanical properties by an increased addition of MiniBars™. The mechanical properties of MiniBars™ FRBC increased more than the geopolymer wtihout MiniBars™: the flexural strength > 11.59-25.97 times, the flexural modulus > 3.33-5.92 times, the tensile strength > 3.50-8.03 times, the tensile modulus > 1.12-1.30 times, and the force load at upper yield tensile strength > 4.18-7.27 times. SEM and optical microscopy analyses were performed on the fractured surface and section of MiniBars™ FRBC and confirmed a good geopolymer network around MiniBars™. Based on our results, MiniBars™ FRBC could be a very promising green material for buildings.
Related Concept Videos
Fiber Reinforced Concrete
Reinforcements in Concrete
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
Abrasion Resistance of Concrete
One such test is the revolving disc test, where three plates...
Mortar Properties