Equation of State of Autoclaved Aerated Concrete-Oedometric Testing

Yuri S Karinski1, Vladimir R Feldgun1, David Z Yankelevsky1,2

  • 1National Building Research Institute, Technion, Haifa 3200003, Israel.

PubMed

Related Concept Videos

Measurement of Air Content in Concrete01:23

Measurement of Air Content in Concrete

Air content measurement in concrete is critical for ensuring structural integrity and durability of concrete structures, especially in environments prone to severe weather conditions. Accurate air content analysis optimizes concrete's resistance to freeze-thaw cycles and enhances its workability and strength. Several methods are standardized under ASTM guidelines to measure the air content in fresh concrete, each suitable for different concrete types and conditions.
The pressure method,...
144
Soundness of Cement01:17

Soundness of Cement

The soundness of cement refers to the ability of cement paste to retain its volume after setting. Unsound cement can lead to expansion and structural damage due to the presence of free lime, magnesia, and calcium sulfate. Free lime hydrates very slowly, expanding and causing unsoundness, which is difficult to detect because it intercrystallizes with other compounds. Magnesia also reacts with water, forming crystals that can disrupt the cement's structure. Calcium sulfate can create...
168
Strength of Cement01:20

Strength of Cement

Strength tests for cement are not performed directly on neat cement paste due to difficulty in obtaining consistent, reliable specimens. Instead, cement is typically tested in the form of cement-sand mortar.
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
137
Porosity and Absorption of Aggregate01:20

Porosity and Absorption of Aggregate

Aggregates contain pores of varying sizes; while some are completely enclosed within the particles, others open onto the surface, allowing water to penetrate. The porosity of aggregates is a major factor contributing to the overall porosity of concrete, given that aggregates constitute about three-quarters of concrete's volume.
When all pores in an aggregate are filled with water, the aggregate is considered saturated and surface-dry. If left in dry air, water will evaporate until the...
287
Effects of Air-entrainment in Concrete01:28

Effects of Air-entrainment in Concrete

Air entrainment in concrete significantly enhances the material's durability, especially in environments subjected to freeze-thaw cycles. Introducing small air bubbles into the concrete mix acts as internal voids that accommodate the expansion of water when it freezes, thereby alleviating internal stress and preventing structural cracks. This function is crucial in climates with significant freezing and thawing, as it protects the concrete from repeated stresses that could lead to premature...
85
Dynamic Modulus of Elasticity of Concrete01:16

Dynamic Modulus of Elasticity of Concrete

The dynamic modulus of elasticity assesses how a concrete structure deforms under impact or dynamic loads. It is typically higher than the static modulus of elasticity, measured under slow, steady loading conditions.
The sonic test is a common method to determine the dynamic modulus. In this test, a concrete beam, sized either 6 x 6 x 30 inches or 4 x 4 x 20 inches, is clamped at its center. Vibrations are initiated at one end of the beam by an electromagnetic exciter unit powered by...