Related Experiment Video
Updated: Apr 14, 2026

In situ Compressive Loading and Correlative Noninvasive Imaging of the Bone-periodontal Ligament-tooth Fibrous Joint
Published on: March 7, 2014
Mechanical insights into jawbone characteristics under chronic kidney disease: A comprehensive nanoindentation
Chie Watanabe1, Jingxiao Zhong2, Sotaro Yamashita3
1Department of Biomaterials and Engineering, Showa University School of Dentistry, Tokyo, Japan.
Abstract:
The mechanical properties of the jawbone play a critical role in determining the successful integration of dental prostheses. Chronic kidney disease (CKD) has been identified to abnormally accelerate bone turnover rates. However, the impact of CKD on the mechanical characteristics of the jawbone has not been extensively studied. This study sought to evaluate the time-dependent viscoelastic behaviors of rat jawbones, particularly in the scenarios both with and without CKD. We hypothesized that CKD might compromise the bone's innate toughening mechanisms, potentially owing to the time-dependent viscoelasticity of the bone matrix proteins. The maxillary and mandibular bones of Wistar rats were subjected to nanoindentation and Raman micro-spectroscopy. Load-hold-displacement curves from the cortical regions were obtained via nanoindentation and were mathematically characterized using a suitable viscoelastic constitutive model. Raman micro-spectroscopy was employed to identify nuanced vibrational changes in local molecular structures induced by CKD. The time course of indenter penetration onto cortical bones during the holding stage (creep behavior) can be mathematically represented by a series arrangement of the Kelvin-Voigt bodies. This configuration dictates the overall viscoelastic response observed during nanoindentation tests. The CKD model exhibited a reduced extent of viscoelastic contributions, especially during the initial ramp loading phase in both the maxillary and mandibular cortical bones. The generalized Kelvin-Voigt model comprises 2 K-Voigt elements that signify an immediate short retardation time (τ1) and a subsequent prolonged retardation time (τ2), respectively. Notably, the mandibular CKD model led to an increase in the delayed τ2 alongside an increase in non-enzymatic collagen cross-linking. These suggest that, over time, CKD diminishes the bone's capability for supplementary energy absorption and dimensional recovery, thus heightening their susceptibility to fractures.
Related Concept Videos
Bone Remodeling
The Functions of the Skeletal System
Bone Disorders
Bone deposition is also affected by the levels of sex hormones like estrogen and testosterone that promote osteoblast activity and bone matrix synthesis. When the level of these hormones decreases due to aging, it causes a reduction in bone deposition. As a result, bone resorption by osteoclasts...
Changes in the Appendicular Skeleton with Age
Initially, the limb buds consist of a core of mesenchyme covered by a layer of ectoderm. The ectoderm at the end of the limb bud thickens to form a narrow crest called the apical ectodermal ridge. This ridge stimulates the underlying...
Introduction to the Skeletal System
Components of the Skeletal System
Bone, or osseous tissue, is a hard connective tissue that forms an internal support structure for the human body. Bones shield vulnerable organs and soft tissue from external forces. For example, the vertebral bones protect and support the spinal cord.
Cartilage, a semi-rigid connective tissue found in regions such as...
Disorders of the Skeletal Muscle
Musculoskeletal disorders
Musculoskeletal disorders involve injuries and conditions affecting the skeletal muscles and associated connective tissues. These disorders can arise from acute biomechanical stresses or chronic overuse and can occur across different age groups. Common injuries include sprains, fractures, and muscular strains, often resulting from...