Enhanced Microwave Deicing Capacity of Cement Pavement with Carbon Fiber Screens

Jiangjiang Li1,2, Peng Zhao1, Minghai Jing1

  • 1School of Materials Science & Engineering, Chang'an University, Xi'an 710061, China.

PubMed

Related Concept Videos

Frost Resistant Concrete01:29

Frost Resistant Concrete

Concrete's susceptibility to frost damage during freeze-thaw cycles demands strategic measures to enhance its frost resistance. Employing techniques like air entrainment, adjusting the water-cement ratio, proper curing, and selecting appropriate aggregates are essential.
Introducing microscopic air bubbles into the concrete mix through air entrainment creates small voids that accommodate ice expansion, thereby reducing internal pressures and preventing cracking. The optimal amount of...
78
Frost Action on Concrete01:27

Frost Action on Concrete

Concrete structures in cold climates, such as those along roadsides, can retain moisture. This moisture makes them susceptible to frost-related damage when temperatures fall below freezing. Adding moisture worsens the damage during temperature fluctuations, leading to repeated freezing and thawing. De-icing salts, spread over these structures to melt ice, add to the freeze-thaw cycle, and draw even more moisture into the concrete.
This freeze-thaw cycle primarily causes surface scaling, where...
97
Fiber Reinforced Concrete01:22

Fiber Reinforced Concrete

Fiber-reinforced concrete significantly enhances the structural and nonstructural properties of traditional concrete by incorporating fibers like steel, glass, and polymers. These fibers, varying from natural ones such as sisal and cellulose to manufactured ones like polypropylene and Kevlar, are mixed into hydraulic cement with aggregates. Steel fibers, often preferred for their robustness, contribute to improved ductility, toughness, and post-cracking performance. The concrete is classified...
75
Effects of Air-entrainment in Concrete01:28

Effects of Air-entrainment in Concrete

Air entrainment in concrete significantly enhances the material's durability, especially in environments subjected to freeze-thaw cycles. Introducing small air bubbles into the concrete mix acts as internal voids that accommodate the expansion of water when it freezes, thereby alleviating internal stress and preventing structural cracks. This function is crucial in climates with significant freezing and thawing, as it protects the concrete from repeated stresses that could lead to premature...
84
Air-entraining Agents01:27

Air-entraining Agents

Air-entraining agents improve the durability and workability of concrete in climates with frequent freezing and thawing. These agents prevent cracks by introducing small air bubbles into the mix, creating spaces accommodating water expansion when temperatures drop. The air-entraining agents lower the surface tension of water, forming stable, small air bubbles. This method is more effective than having accidental large voids, as the intentional, smaller, and evenly distributed air voids improve...
76
Additives and Fillers in Concrete01:29

Additives and Fillers in Concrete

Additives and fillers are integral to enhancing the properties of concrete. Pozzolans and blast-furnace slag are additives or admixtures due to their reactions with calcium hydroxide released during cement hydration. Fillers, which are finely ground and similar in fineness to Portland cement, improve concrete attributes such as workability density, and reduce capillary bleeding or cracking. Some fillers possess hydraulic properties or participate in benign reactions within the cement paste.