Effect of polymerisation protocols on water sorption, solubility and hygroscopic expansion of fast-cure bulk-fill
Halah Thanoon1, Nikolaos Silikas2, David C Watts3
1Division of Dentistry, School of Medical Sciences, University of Manchester, Manchester, UK; Department of Restorative Dentistry, College of Dentistry, King Abdulaziz University, Jeddah, Saudi Arabia.
Objective:
This study examines the effect of two light-curing protocols from a LED polywave light curing unit (LCU) on water sorption, solubility, and hygroscopic expansion of fast and conventional bulk-fill resin-based composites (RBCs) aged in distilled water for 120 d.
Methods:
Three bulk-fill RBCs materials were studied: Tetric PowerFill® (fast photo-polymerised composite) (TPF), Tetric EvoCeram bulk-fill (EVO), and GrandioSo x-tra bulk-fill (GSO) (conventional photo-polymerised composites). Specimens were prepared within a 3D-printed resin mold (8-mm diameter x 4-mm height) and light-cured from one side only with 2 modes of polywave LCU (Bluephase® PowerCure): 3 s mode and for 20 s in "Standard" mode. Water sorption and solubility were measured at fixed time intervals for 120 d of distilled water storage, then reconditioned to dry to measure desorption for 75 d, all at 37 ± 1 °C. Hygroscopic (volumetric) expansion was recorded at the same time intervals up to 120 d. Data were analysed through SPSS using Two-way ANOVA, One-way ANOVA, independent t-tests, and Tukey's post-hoc correction tests (p < 0.05).
Results:
TPF, when irradiated for 3 s demonstrated minimal water sorption (0.83%), solubility (1.01 μg/mm3), and least volumetric expansion (1.64%) compared to EVO and GSO. While EVO showed the highest water sorption (1.03%) and solubility (1.95 μg/mm3) at 3 s. GSO had the lowest sorption (0.67%) and (0.56%) in 3 s and 20 s protocols, respectively. Nevertheless, all the sorption and solubility data were within the ISO 4049 limits.
Significance:
For TPF, fast (3 s) polymerisation did not increase either water sorption or solubility, compared with 20 s irradiation. However, with the two comparative bulk-fill composites, fast cure increased water sorption by 15-25% and more than doubled solubility. These findings were consistent with the lesser volumetric expansions observed for Tetric PowerFill at both the fast and standard protocols, indicating its relative stability across polymerisation protocols.
More Related Videos
Related Concept Videos
Molecular Weight of Step-Growth Polymers
As the step-growth polymerization involves step-wise condensation of monomers, the molecular weight also builds up eventually. Consequently, high molecular weight polymers are obtained at the late stages of the polymerization, where 99% of monomers have been consumed.
The extent of the...
Curing of Concrete
Polymers
Step-Growth Polymerization: Overview
Many natural and synthetic polymers are produced by...
Porosity in Cement Paste
The balance of water to cement in the mix is...
Polymers: Molecular Weight Distribution