Metal Corrosion and the Efficiency of Corrosion Inhibitors in Less Conductive Media
Published on: November 3, 2018
Exploration of rice husk ash as a green corrosion inhibitor immersed in NH4Cl 7.5 % solution
Agus Paul Setiawan Kaban1, Johny Wahyuadi Soedarsono1, Mochammad Syaiful Anwar2
1Prof Johny Wahyuadi Laboratory, Department of Metallurgical and Materials Engineering, Universitas Indonesia, Depok, 16424, Indonesia.
Abstract:
The study reports the development of a liquid smoke solution of rice husk ash (RHA) as a green corrosion inhibitor in NH4Cl solution in approaching corrosion protection for refinery facilities. The recent utilization of RHA has a partial solution to address the possible chemical to form a filming layer to disconnect bare metal and their environment. This work prepared the RHA solution by condensing the RHA vapor before adding it to various concentrations. The corrosion test of potentiodynamic and electrochemicals intends to discover the inhibitor's corrosion resistance before examining the electronic transition corresponding to the contribution of several functional groups using Ultraviolet Visible (UV-Vis) and Fourier-Transform Infrared Spectroscopy (FTIR). Surface evaluation intends to unveil the nature of the corrosion by utilizing the Scanning Electronic and Atomic Force Microscope. The corrosion test result shows the depression of corrosion rate to 0.120 mmpy with high efficiency beyond 96 % in the addition of 7.5 ppm RHA inhibitor. The greater Nyquist semicircle diameter at high concentrations increases the adsorption of the RHA on the surface of C1018. The electronic transition of n-π* and π -π* shows an extensive contribution of C[bond, double bond]C, C[bond, double bond]O, and -OH based on the UV-Vis and FTIR test. The formation of a complex compound of Fe-(NH4Cl-RHA)n blocks the corrosion active sites to reduce the corrosion. This study paves the way for using RHA as an organic compound under NH4Cl conditions, such as in a refinery process facility.
More Related Videos
10:00Experimental Protocol to Determine the Chloride Threshold Value for Corrosion in Samples Taken from Reinforced Concrete Structures
Published on: August 31, 2017
07:44Determining the Chemical Composition of Corrosion Inhibitor/Metal Interfaces with XPS: Minimizing Post Immersion Oxidation
Published on: March 15, 2017
Related Concept Videos
Sample Preparation for Analysis: Advanced Techniques
Acid digestion with strong acids is commonly used to dissolve inorganic materials that are insoluble (do not dissolve) in water. This method can be useful for...
Corrosion of Reinforcement
However, over time and under certain conditions like carbonation, chloride ingress, and cracking this protective state can be compromised. Steel has areas with...
Titration of a Weak Base with a Strong Acid
Using the ICE table and substituting the Kb value, we calculate the initial pH of 50 mL of 0.1 M ammonia to be 11.11. Addition of 25 mL of 0.1 M hydrochloric acid to this solution of ammonia results in a buffer with an equal concentration of ammonia and ammonium ions. The pH of this buffer can be calculated by substituting these...