Biomechanical consideration in tooth-supported glass-ceramic restorations: A systematic review and meta-analysis of survival rates and irreparable failures
Related Experiment Video
Updated: Jul 23, 2026

In situ Compressive Loading and Correlative Noninvasive Imaging of the Bone-periodontal Ligament-tooth Fibrous Joint
Published on: March 7, 2014
Brunna M Ferrairo1, Lucas José de Azevedo-Silva2, Pedro R Minim2
1Postgraduate student, Department of Operative Dentistry, Endodontics and Dental Materials, Bauru School of Dentistry, University of São Paulo (USP), Bauru, Brazil.
Statement Of Problem:
Knowledge on the biomechanical behavior of glass-ceramics, their survival rate over time, and their potential failures is essential for decision-making in clinical practice. Systematic reviews and meta-analysis of their survival rates and irreparable failures are lacking.
Purpose:
The purpose of this systematic review and meta-analysis was to evaluate the survival rates and irreparable failures of various monolithic glass-ceramic dental restorations to help determine biomechanical indications.
Material And Methods:
A comprehensive literature search was conducted across the PubMed, Scopus, Web of Science, and EMBASE databases based on the population, intervention, comparison, and outcome (PICO) question, risk of bias assessment, data extraction, subgroup analysis, and meta-analysis. Both randomized and nonrandomized clinical trials that reported survival rate and irreparable failure were screened. The risk, with a 95% confidence interval, was calculated by using the Mantel-Haenszel method.
Results:
A total of 46 articles met the inclusion criteria: 8 for laminate veneers, 20 for partial coverage restorations, 11 for single crowns, and 6 for fixed partial dentures, encompassing 1715 participants rehabilitated with 4209 restorations. The estimated cumulative survival rate for partial coverage restorations was 90% over an average span of 6.2 years, with an irreparable failure occurrence of n=5.9. Laminate veneers had a survival rate of 90.2% over 6.5 years, with an irreparable failure occurrence of n=8.2. Single crowns had a survival rate of 96% over 4.6 years and an irreparable failure of n=2.7. Conversely, fixed partial dentures had a survival rate of 76.1% over 6.5 years with an irreparable failure of n=5.2.
Conclusions:
Glass-ceramic materials demonstrate relatively high survival rates, indicating that they provide a safe and reliable option for partial coverage restorations, laminate veneers, and single crowns. However, fixed partial dentures had a higher proportion of irreparable failures and a lower survival rate, and caution is required.
Related Concept Videos
Overview of Regeneration and Repair
Regeneration
All animals have varying degrees of...
Teeth
In the bud stage, the tooth germ (an aggregation of cells) starts to form in the developing jawbone. During the cap stage, the tooth germ differentiates into enamel organ, dental papilla, and dental sac, which will later develop into the tooth's enamel, dentin and...