Research on Low-Cost High-Viscosity Asphalt and Its Performance for Porous Asphalt Pavement
Lei Xia1, Qidong Su2, Lingyan Shan2
1School of Materials Science and Engineering, Chang'an University, Xi'an 710061, China.
Abstract:
To develop a cost-effective, high-viscosity asphalt for porous asphalt pavement, we utilized SBS, tackifier, and solubilizer as the main raw materials, identified the optimal composition through an orthogonal experiment of three factors and three levels, and prepared a low-cost high-viscosity asphalt. We compared its conventional and rheological properties against those of rubber asphalt, SBS modified asphalt, and matrix asphalt, employing fluorescence microscopy and Fourier transform infrared spectroscopy for microstructural analysis. The results indicate that the optimal formula composition for high-viscosity asphalt was 4-5% styrene-butadiene-styrene (SBS) + 1-2% tackifier +0-3% solubilizer +0.15% stabilizer. The components evenly dispersed and the performances were enhanced with chemical and physical modification. Compared with SBS modified asphalt, rubber asphalt, and matrix asphalt, the softening point, 5 °C ductility, and 60 °C dynamic viscosity of high-viscosity asphalt were significantly improved, while the 175 °C Brookfield viscosity was equivalent to SBS modified asphalt. In particular, the 60 °C dynamic viscosity reaches 383,180 Pa·s. Rheological tests indicate that the high- and low-temperature grade of high-viscosity asphalt reaches 88-18 °C, and that high-viscosity asphalt has the best high-temperature resistance to permanent deformation and low-temperature resistance to cracking. It can save about 30% cost compared to commercially available high-viscosity asphalt, which is conducive to the promotion and application of porous asphalt pavement.
Related Concept Videos
Masonry Paving
Porosity in Cement Paste
The balance of water to cement in the mix is...
Design Example: Joints in Concrete Pavements
Contraction joints are typically formed by sawing a groove into the concrete shortly after it has hardened. This creates a weakened vertical plane, deliberately encouraging cracking at...
Abrasion Resistance of Concrete
One such test is the revolving disc test, where three plates...
Types of Cement I
Type I (Ordinary Portland Cement) is widely used for general construction where special properties are not required. It has moderate sulfate resistance and heat of hydration.
Type II (Modified Cement) offers moderate resistance to sulfate attack and a lower rate of heat development compared to Type I. It is suitable for structures in...
Porosity and Absorption of Aggregate
When all pores in an aggregate are filled with water, the aggregate is considered saturated and surface-dry. If left in dry air, water will evaporate until the...