Utilizing combusted PET plastic waste and biogenic oils as efficient pour point depressants for crude oil
Mohamed Mohamady Ghobashy1, A M Rashad2, S K Attia2
1Radiation Research of Polymer Chemistry Department, National Centre for Radiation Research and Technology (NCRRT), Egyptian Atomic Energy Authority (EAEA), Cairo, Egypt. ghobashy_ghobashy@yahoo.com.
Abstract:
The deposition of paraffin on pipelines during crude oil transit and low-temperature restart processes poses a significant challenge for the oil industry. Addressing this issue necessitates the exploration of innovative materials and methods. Pour point depressants (PPDs) emerge as crucial processing aids to modify paraffin crystallization and enhance crude oil flow. This study focuses on the combustion of polyethylene terephthalate (PET) waste, a prevalent plastic, in two distinct oils (castor and jatropha). The resulting black waxy substances (PET/Castor and PET/Jatropha) were introduced in varying weights (1000, 2000, and 3000 ppm) to crude oil. The PET/castor oil combination demonstrated a remarkable reduction in pour point from 18 to -21 °C at 3000 ppm concentration, significantly more effective than PET/jatropha blends. Substantial decreases in viscosity (up to 75%) and shear stress (up to 72%) were also observed for both blends, most prominently at lower temperatures near the pour point. The synergistic effect of PET and oils as nucleating agents that alter crystallization patterns and restrict crystal growth contributes to this enhanced low-temperature flow. This highlights the potential of PET plastic waste as an economical, abundant, and eco-friendly additive to develop high-performance PPDs for crude oil.
More Related Videos
Related Concept Videos
Bioremediation
Types of Step-Growth Polymers: Polyesters
Polyesters are commonly prepared from terephthalic acid and ethylene glycol; the crude product is known as poly(ethylene terephthalate) or PET. However, polyesters are synthesized industrially by transesterification of dimethyl terephthalate with ethylene glycol at 150 °C. The two reactants and the...