Related Experiment Video
Updated: May 2, 2026

In situ Compressive Loading and Correlative Noninvasive Imaging of the Bone-periodontal Ligament-tooth Fibrous Joint
Published on: March 7, 2014
In Vitro Effect of Luting Cement on Fracture Resistance of Primary Maxillary Central Incisors with Fiber Posts
Zahra Bahrololoomi1, Alireza Danesh Kazemi2, Fatemeh Zarebidoki1
1Department of Pedodontics, Faculty of Dentistry, Shahid Sadoughi University of Medical Sciences, Yazd, Iran.
Abstract:
Objectives: The use of fiber posts in endodontically treated primary maxillary central incisors improves the retention of composite resin restorations. The purpose of this study was to evaluate the effect of 4 different luting cements on fracture resistance of primary maxillary central incisors with fiber posts. Materials and Methods: In this in vitro study, 40 primary maxillary central incisors were endodontically treated and obturated with Metapex. They were then randomly divided into four groups (n=10) for cementation of fiber posts with GC Fuji I glass ionomer luting cement, Panavia F2.0 dual-cure luting cement, Panavia SA Luting Plus cement (self-adhesive), and TotalCem self-adhesive cement. After 1000 thermal cycles, the fracture resistance was measured. Data were statistically analyzed using ANOVA (alpha=0.05). Results: The mean fracture resistance was 267.07±130.01N in TotalCem, 257.27±102.56N in Panavia F2.0 dual-cure cement, 227.82±110.40N in Panavia SA Luting Plus self-adhesive cement, and 220.89±59.96N in GC Fuji I glass ionomer group. There was no statistically significant difference in fracture resistance among the four groups (P=0.714). Conclusion: Type of luting cement had no significant effect on fracture resistance of primary maxillary central incisors with fiber posts. Nonetheless, TotalCem yielded the highest fracture resistance. Considering its self-adhesive property and easy workability, it can be a good option for cementation of fiber posts in endodontically treated primary central incisors.
More Related Videos
06:16Author Spotlight: Establishing an Accurate Microhardness Testing Protocol for Craniofacial Tissues
Published on: April 26, 2024
07:42Quasistatic Mechanical Testing for Computer-Aided Design and Manufacturing Occlusal Veneers Cemented to Milled Dentin Analog Material
Published on: December 20, 2024
Related Concept Videos
Stress-Strain Diagram - Brittle Materials
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
Tensile Strength Considerations of Concrete
The dimensions and shape of a concrete specimen...
Behavior of Concrete Under Compressive Load
As the concrete specimen fractures under...