Impact of Water-Cement Ratio on Concrete Mechanical Performance: Insights into Energy Evolution and Ultrasonic Wave

Junzhi Lin1,2,3, Bincheng Tian1,2,3, Zelong Liang2,4

  • 1Key Laboratory of Hydraulic and Waterway Engineering of the Ministry of Education, Chongqing Jiaotong University, Chongqing 400074, China.

PubMed

Related Concept Videos

Water Cement Ratio01:28

Water Cement Ratio

The water-cement ratio is pivotal in defining concrete's quality. This ratio, a balance between the weight of water and cement in the mix, shapes the concrete's strength, durability, and resistance to environmental factors. As identified by Abrams’ law, less water in the mix equates to stronger concrete. However, water is essential not only for the chemical process of hydration but also for the concrete's workability and compaction. While hydration chemically binds water and...
541
Curing of Concrete01:20

Curing of Concrete

The hydration of cement takes place within the water-filled capillary pores. However, environmental elements can disrupt this process by evaporating water from the concrete surfaces. Sealed concrete with a water-cement ratio below 0.5 experiences self-desiccation, leading to water loss. The water loss in concrete is mitigated by curing. This technique involves keeping the concrete saturated to maintain the necessary temperature and moisture conditions, to optimally fill the spaces in the cement...
89
Effect of Sea Water on Concrete01:22

Effect of Sea Water on Concrete

Concrete exposed to seawater can undergo degradation like the dissolution of ettringite and gypsum, increasing the material's porosity and decreasing its strength. In contrast, the crystallization of salts within the concrete's pores can cause expansion, particularly above the waterline where evaporation occurs. Nonetheless, this expansion only happens when seawater, enabled by the concrete's permeability, manages to infiltrate the structure.
Concrete in areas between tide marks,...
206
Testing Water Quality01:14

Testing Water Quality

When the quality of water for concrete preparation is uncertain, its impact on the setting time of cement and compressive strength of mortar is assessed by comparison with de-ionized or distilled water benchmarks. American Society for Testing and Materials (ASTM) C1602 requires the setting times to be within 90 minutes of the control, British Standard (BS) 3146:1980 allows a 30-minute variance in the initial setting, while British Standards European Norm (BS EN) 1008 specifies initial setting...
103
Quality of Water01:19

Quality of Water

In concrete preparation, the quality of water is paramount as it affects the strength and durability of the concrete. Potable water is usually preferred; however, it must not have excessive sodium or potassium to prevent compromising the concrete's integrity. Water quality is typically evaluated based on impurities such as dissolved solids, chlorides, and sulfates, and its pH value is ideally between 6 and 8. Even slightly acidic natural water may be acceptable unless it contains harmful...
89
Permeability of Concrete01:25

Permeability of Concrete

Permeability in the context of concrete refers to how easily liquids or gases can pass through the material. This quality is crucial for assessing the water-tightness and durability of concrete structures and their resistance to chemical attacks. Concrete permeability can be determined through comparative laboratory tests. These tests typically involve sealing a concrete specimen from the sides, applying water pressure to the top surface with pressure, and measuring the amount of water passing...
131