Related Experiment Video
Updated: Jun 17, 2025

Additive Manufacturing of Functionally Graded Ceramic Materials by Stereolithography
Published on: January 25, 2019
The Diatomite Grinding Technology Concept for the Protection of Diatomite Shells and the Control of Product Grading
Agata Stempkowska1, Tomasz Gawenda1, Krzysztof Smoroń2
1Faculty of Civil Engineering and Resource Management, Department of Environmental Engineering, AGH University, Mickiewicza 30 Av., 30-059 Kraków, Poland.
Abstract:
Diatomite deposits in Poland are located in the Podkarpackie Voivodeship, and the only active deposit is in Jawornik Ruski. Therefore, it is a unique material. Improved rock processing methods are constantly in demand. In the research presented here, we have used research methods such as X-ray diffraction (XRD), scanning electron microscope (SEM), particle shape analysis, and appropriate sets of crushing machines. Diatomite comminution tests were carried out on test stands in different crushers (jaw crusher, hammer crusher, high-pressure roller press, ball mill) using different elementary crushing force actions: crushing, abrasion, and impact, occurring separately or in combination. The machines were tested with selected variable parameters to obtain products with a wide range of grain sizes ranging from 0 to 10 mm. The ball mill (yield 87%, system C3) and the hammer crusher with HPGR (high-pressure grinding roller) (yield 79%, system D2 + D3) have the greatest impact on diatom shell release and accumulation in the finest 0-5 μm and 5-10 μm fractions. For commercial purposes, it is important to obtain very fine fractions while keeping the shells undisturbed.
Related Concept Videos
Deleterious Substances in Aggregate
Another type of impurity is clay and fine material that...
Abrasion Resistance of Concrete
One such test is the revolving disc test, where three plates...
Design Example: Aggregate Gradation
The grading, or particle-size distribution, of sand is determined using sieve analysis, with standard sizes ranging from 150 μm to 10 mm (ASTM No. 100 sieve to 3⁄8 in. sieve). Sand is...