Comparative Study of the Foaming Behavior of Ethylene-Vinyl Acetate Copolymer Foams Fabricated Using Chemical and
Yaozong Li1, Junjie Jiang1, Hanyi Huang1
1School of Materials Science and Engineering, Sun Yat-sen University, Guangzhou 510275, China.
Abstract:
Ethylene-vinyl acetate copolymer (EVA), a crucial elastomeric resin, finds extensive application in the footwear industry. Conventional chemical foaming agents, including azodicarbonamide and 4,4'-oxybis(benzenesulfonyl hydrazide), have been identified as environmentally problematic. Hence, this study explores the potential of physical foaming of EVA using supercritical nitrogen as a sustainable alternative, garnering considerable interest in both academia and industry. The EVA formulations and processing parameters were optimized and EVA foams with densities between 0.15 and 0.25 g/cm3 were produced. Key findings demonstrate that physical foaming not only reduces environmental impact but also enhances product quality by a uniform cell structure with small cell size (50-100 μm), a wide foaming temperature window (120-180 °C), and lower energy consumption. The research further elucidates the mechanisms of cell nucleation and growth within the crosslinked EVA network, highlighting the critical role of blowing agent dispersion and localized crosslinking around nucleated cells in defining the foam's cellular morphology. These findings offer valuable insights for producing EVA foams with a more controllable cellular structure, utilizing physical foaming techniques.
More Related Videos
08:38Microfluidic Devices for Characterizing Pore-scale Event Processes in Porous Media for Oil Recovery Applications
Published on: January 16, 2018
10:06Microfluidic Fabrication Techniques for High-Pressure Testing of Microscale Supercritical CO2 Foam Transport in Fractured Unconventional Reservoirs
Published on: July 2, 2020
Related Concept Videos
Molecular Weight of Step-Growth Polymers
As the step-growth polymerization involves step-wise condensation of monomers, the molecular weight also builds up eventually. Consequently, high molecular weight polymers are obtained at the late stages of the polymerization, where 99% of monomers have been consumed.
The extent of the...
Free-Radical Chain Reaction and Polymerization of Alkenes
Physical Properties of Ethers
An ether molecule has a net dipole moment due to the polarity of C–O bonds. Subsequently, boiling points of ethers are lower than those of alcohols of comparable molecular weight and slightly higher than those of hydrocarbons of comparable molecular weight (Table 1).
Ethers can act as hydrogen bond acceptors, making them more water-soluble than hydrocarbons, but since ethers cannot act as hydrogen bond donors, they are much less soluble in water than alcohols. Ethers are considered...
Polymer Classification: Stereospecificity
Anionic Chain-Growth Polymerization: Overview