Related Experiment Video
Updated: Jun 13, 2025

Preparation of Aligned Steel Fiber Reinforced Cementitious Composite and Its Flexural Behavior
Published on: June 27, 2018
Experimental and Numerical Investigation of the Flexural Behavior of Reinforced-Concrete Beams Utilizing Waste
Fuat Korkut1, Memduh Karalar2, Ali Motameni3
1Department of Civil Engineering, Van Yüzüncü Yıl University, Van 65090, Turkey.
Abstract:
During the process of cutting andesite stones, the waste mud is kept in powder form once fully dried. It is difficult to store the waste that is produced as a consequence of the extensive utilization area and consumption of andesite. Thus, eliminating waste storage challenges and incorporating these wastes into the economy are crucial. For this reason, this study examined the effects of waste andesite dust (WAD) on the flexural behavior of reinforced-concrete beams (RCBs) using experimental testing and 3D finite-element modeling (FEM) via ANSYS. Thus, different rates of WAD up to 40% were used to investigate the influence of the WAD rate on the fracture and bending behavior of RCBs. While the RCB with 10% WAD had a slightly lower load-bearing and ductility capacities, ductility capacities significantly drop after 10% WAD. At 40% WAD, both the load-bearing capacity and ductility significantly reduced. Based on the experimental findings, using 10% WAD as a replacement for cement is a reasonable choice to obtain eco-friendly concrete. Moreover, the outcomes of 3D FEM were also compared with those of experiments conducted using ANSYS v19 software. The displacement values between the test and FEM findings are quite similar.
Related Concept Videos
Fiber Reinforced Concrete
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
Abrasion Resistance of Concrete
One such test is the revolving disc test, where three plates...
Dynamic Modulus of Elasticity of Concrete
The sonic test is a common method to determine the dynamic modulus. In this test, a concrete beam, sized either 6 x 6 x 30 inches or 4 x 4 x 20 inches, is clamped at its center. Vibrations are initiated at one end of the beam by an electromagnetic exciter unit powered by...
Shrinkage in Concrete
When concrete is still in its plastic state, it can undergo a decrease in volume by about 1% of its absolute volume. This decrease is known as plastic shrinkage. It arises either...
Additives and Fillers in Concrete
The...