Related Experiment Video
Updated: May 10, 2026

Electron Channeling Contrast Imaging for Rapid III-V Heteroepitaxial Characterization
Published on: July 17, 2015
The Influence of Etching Method on the Occurrence of Defect Levels in III-V and II-VI Materials
Kinga Majkowycz1, Krzysztof Murawski1, Małgorzata Kopytko1
1Institute of Applied Physics, Military University of Technology, 2 Kaliskiego St., 00-908 Warsaw, Poland.
Abstract:
The influence of the etching method on the occurrence of defect levels in InAs/InAsSb type-II superlattice (T2SLs) and MCT photodiode is presented. For both analyzed detectors, the etching process was performed by two methods: wet chemical etching and dry etching using an ion beam (RIE-reactive ion etching). The deep-level transient spectroscopy (DLTS) method was used to determine the defect levels occurring in the analyzed structures. The obtained results indicate that the choice of etching method affects the occurrence of additional defect levels in the MCT material, but it has no significance for InAs/InAsSb T2SLs.
Related Concept Videos
Imperfections in Crystal Structure: Point, Line and Plane Defects
Imperfections in Crystal Structure: Stoichiometric Point Defects
Imperfections in Crystal Structure: Non-Stoichiometric Defects