Analysis of differential scanning calorimetry data for aged plutonium
1Los Alamos National Laboratory, P.O. Box 1663, Los Alamos, New Mexico 87544, USA.
Abstract:
Differential scanning calorimetry data for samples of a 52 year old plutonium alloy with 3.3 at. % Ga that were heated beyond the melting point is analyzed using transition state theory to find activation energies for the δ to ɛ and ɛ to liquid phase transitions. A Bayesian statistical method involving a Gaussian process model is used to find mean values and confidence intervals for the activation energies. The activation energy for the δ to ɛ phase transition increases by 3.3 ± 3.8% per decade, relative to the case when all age related plutonium lattice point defects have been removed through annealing. The corresponding increase in activation energy for the ɛ to liquid transition is shown to be 7.1 ± 1.8% per decade. It is postulated that the change in activation energy with age for both phase transitions is caused, in part, by the accumulation of the same type of lattice point defects associated with the observed increase in elastic bulk modulus over time.
More Related Videos
09:18Laser-heating and Radiance Spectrometry for the Study of Nuclear Materials in Conditions Simulating a Nuclear Power Plant Accident
Published on: December 14, 2017
08:13Differential Scanning Calorimetry — A Method for Assessing the Thermal Stability and Conformation of Protein Antigen
Published on: March 4, 2017