Aluminum-Doped Indium Oxide Electron Transport Layer Grown by Atomic Layer Deposition: Highly Efficient and

Pil Ju Youn1, Mun Young Woo2, Jong Hyeon Won1

  • 1Department of Materials Science and Engineering, Seoul National University of Science and Technology, Seoul, 01811, Republic of Korea.