Scalable robust photothermal superhydrophobic coatings for efficient anti-icing and de-icing in simulated/real
Mingyuan Mao1, Jinfei Wei1, Bucheng Li1
1Center of Resource Chemistry and Energy Materials, Key Laboratory of Clay Mineral of Gansu Province, and State Key Laboratory of Solid Lubrication, Lanzhou Institute of Chemical Physics, Chinese Academy of Sciences, Lanzhou, PR China.
Abstract:
Photothermal superhydrophobic coatings are supposed promising to prevent ice accumulation on infrastructures but often experience significant performance degradation in real icing conditions and lack mechanical robustness. Here, we report design of robust photothermal superhydrophobic coatings with three-tier hierarchical micro-/nano-/nanostructures by deposition of nanosized MOFs on natural attapulgite nanorods, fluorination, controlled phase separation of a hydrophobic adhesive and spraying assembly. Phase separation degree and adhesive content significantly influence the coatings' properties by regulating the structural parameters and morphology. In simulated/real icing environments, the coatings simultaneously show (i) high superhydrophobicity and stable Cassie-Baxter states due to their low-surface-energy, three-tier micro-/nano-/nanostructure, (ii) excellent photothermal effect primarily due to nanosized MOFs, and (iii) good mechanical robustness by the phase-separated adhesive, reinforcement with attapulgite and the coatings' self-similar structure. Accordingly, combined with low thermal conductivity, the coatings exhibit remarkable anti-icing/frosting (e.g., no freezing in at least 150 min and almost free of frost in 25 min) and de-icing/frosting performances (e.g., fast de-icing in 12.7 min and fast de-frosting in 16.7 min) in such environments. Furthermore, we realize large-scale preparation of the coatings at reasonable costs. The coatings have great application potential for anti-icing and de-icing in the real world by efficiently using natural sunlight.
More Related Videos
Related Concept Videos
Thermal Expansion
Cold Weather Concreting
To counteract the negative impacts of cold weather, ensuring...
Frost Action on Concrete
This freeze-thaw cycle primarily causes surface scaling, where...
Frost Resistant Concrete
Introducing microscopic air bubbles into the concrete mix through air entrainment creates small voids that accommodate ice expansion, thereby reducing internal pressures and preventing cracking. The optimal amount of entrained...