Related Experiment Video
Updated: Jun 7, 2025

Atomically Traceable Nanostructure Fabrication
Published on: July 17, 2015
Design of an atomic layer deposition system with in situ reflection high energy electron diffraction
Alexandra J Howzen1, Justin Caspar2, Alparslan Oztekin2
1Department of Materials Science and Engineering, Lehigh University, Bethlehem, Pennsylvania 18015, USA.
Abstract:
We report the design, fabrication, and testing of an atomic layer deposition (ALD) system that is capable of reflection high energy electron diffraction (RHEED) in a single chamber. The details and specifications of the system are described and include capabilities of RHEED at varied accelerating voltages, sample rotation (azimuthal) control, sample height control, sample heating up to set temperatures of 1050 °C, and either single- or dual-differential pumping designs. Thermal and flow simulations were used to justify selected system dimensions as well as carrier gas/precursor mass flow rates. Temperature calibration was conducted to determine actual sample temperatures that are necessary for meaningful analysis of thermally induced transitions in ALD thin films. Several demonstrations of RHEED in the system are described. Calibration of the camera length was conducted using a gold thin film by analyzing RHEED images. Finally, RHEED conducted at a series of increasing temperatures was used to monitor the crystallization of an ALD HfO2 thin film. The crystallization temperature and the ring pattern were consistent with the monoclinic structure as determined by separate x-ray diffraction-based measurements.
More Related Videos
07:24Quantitative Atomic-Site Analysis of Functional Dopants/Point Defects in Crystalline Materials by Electron-Channeling-Enhanced Microanalysis
Published on: May 10, 2021
14:11Quantification of Hydrogen Concentrations in Surface and Interface Layers and Bulk Materials through Depth Profiling with Nuclear Reaction Analysis
Published on: March 29, 2016
Related Concept Videos
Atomic Emission Spectroscopy: Instrumentation
Inductively Coupled Plasma Atomic Emission Spectroscopy: Instrumentation
There are three main types of inductively coupled plasma atomic emission spectroscopy (ICP-AES) instruments: sequential, simultaneous multichannel, and Fourier transform instruments, with the latter being less commonly used....