Related Experiment Video
Updated: Jun 5, 2025

Zinc-Sponge Battery Electrodes that Suppress Dendrites
Published on: September 29, 2020
Microscopic Insights into Zn (002) Epitaxial Electrodeposition in Aqueous Zinc Metal Batteries
Chunyu Zhao1, Jie Sun1, Wencheng Lu2
1Key Laboratory of Physics and Technology for Advanced Batteries (Ministry of Education), College of Physics, Jilin University, Changchun 130012, China.
Abstract:
Dendrite growth, corrosion, passivation, and other side reactions during Zn plating and stripping have consistently hindered the capacity and lifespan of Zn metal batteries. In this study, we employ first-principles calculations to unravel the epitaxial electroplating mechanism of Zn (002) planes on various substrate surfaces. We identify six critical factors, including interfacial stability, zincophilicity, surface atomic arrangement, lattice mismatch, responsiveness, and adaptability, that profoundly influence the electrochemical behavior of zinc deposition. Our findings reveal that substrates with hexagonal surface atomic arrangements and strong metallic bonding with zinc, such as (002)-Zn, (111)-Cu, and Ti3C2 MXenes, facilitate uniform and dendrite-free zinc deposition. Notably, lattice contraction induced by substrate lattice mismatch exerts a greater impact on the deposition stability than lattice expansion. Kinetic analyses demonstrate that substrates exhibiting high responsiveness and adaptability can tolerate higher current densities and larger areal capacities, which are crucial for practical applications.
Related Concept Videos
Standard Electrode Potentials
Electrodeposition
Electrodeposition can...