The Effect of Preheating on the Mechanical Properties of AISI 1037 and AISI 304 Welded Joints Using Shielded Metal
Sudarsono1, Amir Arifin2, Gunawan2
1Mechanical Engineering Department, Halu Oleo University, Kendari 93232, Indonesia.
Abstract:
This study explores the effect of preheating on the toughness of dissimilar welded joints between AISI 1037 and AISI 304 steels, using Shielded Metal Arc Welding (SMAW) and E309-16 electrodes. The innovation of this approach lies in assessing how preheating temperatures influence the mechanical properties of such welds. Preheating temperatures ranged from 150 °C to 300 °C, with impact testing revealing a notable increase in toughness, from 6.01 Joules at 150 °C to 19.57 Joules at 300 °C. Hardness tests indicated a maximum hardness of 313 VHN in the fusion zone and a minimum of 185 VHN in the AISI 304 area. Compared to non-preheated joints, preheating significantly enhanced impact strength and altered the fracture mode from brittle to ductile. Macrostructural and microstructural analyses with optical microscopy and SEM showcased changes in fracture surfaces and microstructural evolution, highlighting the improvement in mechanical properties due to preheating. These findings demonstrate that preheating critically enhances the toughness and overall performance of dissimilar metal welds, making it a valuable technique in industrial applications where enhanced joint toughness is crucial.
Related Concept Videos
Residual Stresses
Mechanical Characteristics of Steel
The tension test is fundamental for determining tensile strength. In this test, a steel specimen is stretched using a gripping device until it breaks. The data collected during this test are used...
Steel Fastening Techniques
Rivets are cylindrical steel fasteners with a specially designed head. During application, rivets are heated until white-hot and then inserted through pre-drilled holes in the steel sections. A pneumatic hammer is used to shape the exposed end into a second head, securing the sections together.
Bolting is another...
Thermal expansion and Thermal stress: Problem Solving
To solve the problem, first, identify the known and unknown quantities. The initial length (L) of the bridge is 1275 m, the coefficient of linear expansion (α) for steel is 12 x 10-6/°C, and the change in...
Structural Steel Products
Once shaped, the steel's final form emerges as a continuous length, which is then segmented by a hot saw into manageable pieces. These segments...
Cold Weather Concreting
To counteract the negative impacts of cold weather, ensuring...