Styrene-Butadiene Rubber Latex Modified Mortars Prepared with High Early Strength Portland Cement
Modestas Kligys1, Giedrius Girskas1
1Institute of Building Materials, Faculty of Civil Engineering, Vilnius Gediminas Technical University (VILNIUS TECH), 10223 Vilnius, Lithuania.
Abstract:
The increased early hydration rate of high early strength cement has economic advantages in many civil engineering fields (faster formwork removal or earlier demoulding of precast elements). Styrene-butadiene rubber (SBR) latex is the most common polymer in aqueous dispersions suitable for admixing in cement-based materials. It allows the designing of structures with specific properties for a variety of applications. The analysis of literature sources has shown that different properties of SBR latex-modified cement-based material samples reported were usually measured at 3, 7, 14, and 28 days of hardening. In this research, the authors decided to investigate a combined effect of high early strength Portland cement, characterized by an increased hydration rate, and SBR latex able to retard this process for a prolonged hardening period-up to 90 days in modified mortar samples. This study covers the results of the effect of different amounts of SBR latex (5%, 10%, 15%, and 20%) on the properties of modified mortar samples with a constant water-to-cement ratio prepared with high early strength Portland cement 42.5 R. The mortar samples were prepared from local raw materials produced by the Lithuanian companies. The properties, such as dry bulk density, ultrasonic pulse velocity, capillary water absorption, compressive and flexural strengths, and toughness, after three different hardening periods (7, 28, and 90 days) of the mortar samples were investigated. The applied mathematical-statistical methods allowed a detailed prognosis of the dependence between the dry bulk density and the strength properties of modified mortar samples. The combination of 42.5 R strength class Portland cement with the SBR latex in amounts ranging from 5% to 20% seems to be suitable for designing durable structures with specific properties.
More Related Videos
05:36Production and Analysis of Sporosarcina pasteurii Biocement Bricks Using Custom 3D-Printed Molds for Unconfined Compression Tests
Published on: March 7, 2025
07:02The Preparation and Properties of Thermo-reversibly Cross-linked Rubber Via Diels-Alder Chemistry
Published on: August 25, 2016
Related Concept Videos
Types of Cement II
Types of Cement I
Type I (Ordinary Portland Cement) is widely used for general construction where special properties are not required. It has moderate sulfate resistance and heat of hydration.
Type II (Modified Cement) offers moderate resistance to sulfate attack and a lower rate of heat development compared to Type I. It is suitable for structures in...
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
Mortar
Superplasticizers
Accelerators
The effectiveness of calcium chloride can...