The Negative Role of Proton Insertion on the Lifetime of Vanadium-Based Aqueous Zinc Batteries
Chaoqiong Zhu1, Limin Zheng1, Hao Ruan1
1School of Chemical Engineering, Sichuan University, Chengdu, 610065, P. R. China.
Abstract:
Vanadium oxides are attracted cathodes for aqueous zinc batteries owing to their high capacity. However, the limited cyclability of vanadium-based oxide cathodes, especially at low current densities, impedes their practical application. Here, it is revealed that proton insertion is responsible for the limited lifetime of vanadium oxides. Proton insertion promotes the dissolution of vanadium oxides, deteriorating electrochemical performance. Propylene carbonate (PC) is introduced into Zn(CF3SO3)2 electrolyte to regulate the coordination environment of water, forming PC-coordinated Zn2+ solvation structure and [H2O-CF3SO3 --PC] complex. The optimized coordination environment of water weakens the adsorption energy between water molecules and vanadium oxides, inhibiting proton insertion. As a result, vanadium-based oxides cathode without proton insertion can maintain the stability of crystal structure and avoid the dissolution of V. Taking CaV8O20·nH2O as cathode, Zn||CaV8O20·nH2O battery without proton insertion performs enhanced cycling performance. This work not only reveals the negative effect of proton insertion on the lifetime of vanadium-based oxides cathode but also provides an effective strategy to modulate proton insertion.
Related Concept Videos
Batteries and Fuel Cells
Standard Electrode Potentials
EDTA: Auxiliary Complexing Reagents
Van de Graaff Generator
Van de Graaff uses both smooth and pointed surfaces, conductors, and insulators to generate large static charges and, hence, large voltages. A substantial excess charge can be deposited on the sphere because it moves...
Voltammetry: Stripping Methods
Anodic Stripping Voltammetry (ASV)
ASV is used to determine metals and metalloids at trace levels. It involves two steps: deposition and stripping. First, a negative potential is applied to the...
Concentration Cells
Consider the following voltaic cell: