Effect of Mo Addition on the Susceptibility of Advanced High Strength Steels to Liquid Metal Embrittlement
Fateme Abdiyan1, Joseph R McDermid1, Fernando Okigami2
1Department of Materials Science and Engineering, McMaster University, Hamilton, ON L8S 4L8, Canada.
Abstract:
Liquid metal embrittlement (LME) in Zn-coated advanced high-strength steels (AHSSs) is an increasing concern, particularly in automotive assembly, where it can cause early failure and reduce ductility during resistance spot welding (RSW). This study explores the impact of adding 0.2 wt% Mo on the LME susceptibility of 0.2C-2Mn-1.5Si AHSS through hot tensile testing, RSW, and advanced microstructural analyses, including atom probe tomography (APT) and transmission electron microscopy (TEM). The results suggest that Mo enhances resistance to LME, as evidenced by the increased tensile stroke from 2 mm in the case of the 0 Mo alloy and to 2.75 mm in the case of the 0.2 Mo sample. Also, the average crack length in the shoulder of the welded samples decreased from 109 ± 7 μm to 28 ± 3 μm by adding 0.2 wt% Mo to the base alloy. APT analysis revealed that, in the presence of Mo, there is increased boron (B) segregation at austenite grain boundaries, improving cohesion, while TEM suggested more diffusion of Zn into the substrate, facilitating the formation of Zn-ferrite. These findings highlight Mo's potential to reduce LME susceptibility of AHSS for automotive applications.
More Related Videos
14:51An Available Technique for Preparation of New Cast MnCuNiFeZnAl Alloy with Superior Damping Capacity and High Service Temperature
Published on: September 23, 2018
08:55Methods of Ex Situ and In Situ Investigations of Structural Transformations: The Case of Crystallization of Metallic Glasses
Published on: June 7, 2018
Related Concept Videos
Bonding in Metals
Mechanical Characteristics of Steel
The tension test is fundamental for determining tensile strength. In this test, a steel specimen is stretched using a gripping device until it breaks. The data collected during this test are used...
Corrosion of Reinforcement
However, over time and under certain conditions like carbonation, chloride ingress, and cracking this protective state can be compromised. Steel has areas with...
Stress-Strain Diagram - Ductile Materials