Related Experiment Video
Updated: Jun 16, 2026

Characterization Of Multi-layered Fish Scales Atractosteus spatula Using Nanoindentation, X-ray CT, FTIR, and SEM
Published on: July 10, 2014
A Brief Introductory Guide to Nanoindentation for Comparative and Evolutionary Biologists, with a Case Study of Bone
D S Adams1, B L Boyce2, D E Hooks3
1Department of Biological Sciences, Clemson University, Clemson, SC 29634, USA.
Abstract:
Quantifying the material properties of hard biological materials can improve understanding of the relationships between form, function, and performance. This study illustrates the use of nanoindentation as a tool for evaluating material properties in a comparative biology framework. We provide a step-by-step guide for comparative and evolutionary biologists illustrating the collection and analysis of nanoindentation data from samples of artiodactyl skull bones. We assess the impact of methodological decisions on the output of nanoindentation tests. We also investigate whether evolutionary variations in skull bone properties are present between artiodactyl species that engage in intraspecific head-to-head combat and those that do not. Elastic modulus exhibited little variation among numbers of indents performed per test and per bone sample. The average elastic modulus was significantly lower when bones were hydrated with deionized water. The skulls of artiodactyls exhibited a gradient of elastic modulus values in which the anterior of the skull is less stiff than more posterior locations. Species involved in head-to-head combat showed little difference in elastic modulus values compared to non-combat species. This suggests that ecological factors influence the evolutionary diversity of bone material properties, rather than strictly phylogenetic constraints. In a phylogenetic context, nanoindentation reveals tetrapod bone heterogeneity and provides insights into the evolution of these traits.
Related Concept Videos
Gross Anatomy of Bone
The diaphysis is the tubular shaft that runs between the proximal and distal ends of the bone. The walls of the diaphysis are composed of dense and hard compact bone made of numerous osteons — the functional unit of the compact bone. The hollow region in the diaphysis is called the medullary cavity, which harbors the bone marrow. In infants and children, this marrow cavity is filled with red marrow, whereas in adults, it...
Overview of the Skull
The cranial vault surrounds and protects the brain and houses the middle and inner ear structures. This cavity is bounded superiorly by the rounded top of the skull, which...