Unravelling electro-chemo-mechanical processes in graphite/silicon composites for designing nanoporous and
Xuekun Lu1,2, Rhodri E Owen3,4, Wenjia Du3,4,5
1School of Engineering and Materials Science, Queen Mary University of London, London, UK. xuekun.lu@qmul.ac.uk.
None:
Silicon is a promising negative electrode material for high-energy batteries, but its volume changes during cell cycling cause rapid degradation, limiting its loading to about 10 wt.% in conventional graphite/Si composite electrodes. Overcoming this threshold requires evidence-based design for the formulation of advanced electrodes. Here we combine multimodal operando imaging techniques, assisted by structural and electrochemical characterizations, to elucidate the multiscale electro-chemo-mechanical processes in graphite/Si composite negative electrodes. We demonstrate that the electrochemical cycling stability of Si particles strongly depends on the design of intraparticle nanoscale porous structures, and the encapsulation and loss of active Si particles result in excessive charging current being directed to the graphite particles, increasing the risk of lithium plating. We also show that heterogeneous strains are present between graphite and Si particles, in the carbon-binder domain and the electrode's porous structures. Focusing on the volume expansion of the electrode during electrochemical cycling, we prove that the rate performance and Si utilization are heavily influenced by the expansion of the carbon-binder domain and the decrease in porosity. Based on this acquired knowledge, we propose a tailored double-layer graphite/Si composite electrode design that exhibits lower polarization and capacity decay compared with conventional graphite/Si electrode formulations.