Plasma-enhanced atomic layer deposition of AlPO4/AlPxOy: comparing dual source and supercycle approaches for composition control
Related Experiment Video
Updated: Jan 11, 2026

Growth and Electrostatic/chemical Properties of Metal/LaAlO3/SrTiO3 Heterostructures
Published on: February 8, 2018
Florian Preischel1,2, David Zanders1, Jean-Pierre Glauber1,2
1Inorganic Materials Chemistry, Ruhr University Bochum, Universitätsstr. 150, 44801 Bochum, Germany.
Abstract:
In pursuit of developing a plasma-enhanced atomic layer deposition (PEALD) process for AlPO4, we explored two different approaches, both employing an O2 plasma as the co-reactant. First-principles density functional theory (DFT) calculations indicate that TMA-phosphine adducts are stable, with ethyl or isopropyl groups on the phosphine. The adducts were thermally characterized, with the newly synthesized [Me3AlPiPr3] (TMAPIP) featuring a promising one-step evaporation. Therefore, it was tested as a dual-source precursor at 120 °C, providing both Al and P atoms for the resulting AlPxOy layers, thereby simplifying the process design. Although the P content of the PEALD-deposited films was limited to a few percent, this might be advantageous for P doping of Al2O3. The second approach, therefore, involved a supercycle (SC) process design, in which the number of phosphorus reagent sub-cycles using P(NMe2)3 as the precursor was varied alongside a single Al2O3 cycle with TMA; in both cases, O2 plasma was used as the co-reactant. Simple gas-phase DFT calculations show that P(NMe2)3 reacts favorably with the chemisorbed Al species present in the second sub-cycle. The SC method enabled the incorporation of significantly higher amounts of P over a broad temperature range from 60 °C to 240 °C. The deposition of stoichiometric AlPO4 was ultimately achieved by varying the number of phosphorus cycles, allowing the composition to be precisely adjusted via the deposition temperature.