The Effect of Anodization Parameters on the Aluminum Oxide Dielectric Layer of Thin-Film Transistors
Published on: May 24, 2020
High-Mobility IZO Thin-Film Transistors Enabled by Precise Hydrogen Control Using a SiO2-Al2O3 Supercycle via
Sunghwan Park1, Seong-In Cho2, Hwa Young Kim1
1Department of Materials Science and Engineering, Korea Advanced Institute of Science and Technology (KAIST), 291 Daehak-ro, Yuseong-gu, Daejeon 305-701, Republic of Korea.
Abstract:
A precise strategy to control hydrogen incorporation is essential for achieving high-performance oxide thin-film transistors (TFTs) as hydrogen plays a key role in tuning carrier concentration and passivating defect states. In this study, we report a top-gate oxide thin-film transistor structure that utilizes a plasma-enhanced atomic layer deposition (PEALD) supercycled SiO2-Al2O3 gate insulator (GI), enabling precise hydrogen control through a tunable layering sequence. Hydrogen incorporation into the active channel is modulated with precise control by varying the number of hydrogen-rich SiO2 subcycles. Comprehensive analyses reveal that moderate hydrogen incorporation effectively passivates oxygen-related defects while introducing shallow donor states, enhancing mobility, and suppressing charge trapping. The optimized device with ten cycles of H-rich SiO2 exhibits a high field-effect mobility of 47.4 cm2/V·s, a turn-on voltage (Von) of -0.46 V, a subthreshold swing of 71.3 mV/dec and negligible hysteresis, an on/off current ratio of ∼107, and superior bias stability under positive and negative stress conditions. In contrast, excess hydrogen from 15 cycles leads to the loss of switching behavior caused by the intermixing of GI layers, resulting in uncontrolled hydrogen diffusion and excessive carrier generation. These results demonstrate that the PEALD supercycle process offers a reliable strategy for hydrogen modulation in oxide semiconductors, enabling an optimized trade-off between mobility and stability in high-performance TFTs.