B3C2N3 monolayer with vacancy defects decorated with lithium as a potential hydrogen storage system: a DFT study
Rezvan Rahimi1,2, Mohammad Solimannejad1,2, Yafei Zhang3
1Department of Chemistry, Faculty of Science, Arak University, Arak 3848177584, Iran. r-rahimi@araku.ac.ir.
None:
This research explores the capability of lithium-modified pristine and defect-engineered B3C2N3 monolayers (VB, VC, and VN) for hydrogen storage, employing periodic DFT calculations. Several key metrics were evaluated, including the adsorption and binding energies of lithium atoms and H2 molecules on these substrates, storage capacity, desorption temperatures, electronic characteristics, and the molecular stability of the structures. The findings reveal that the most thermodynamically favorable configuration comprises eight lithium atoms, yielding an optimal adsorption energy of -0.199 eV per H2 molecule in the final state, designated as 20H2@8Li-VC. This configuration further exhibits a gravimetric hydrogen storage capacity of 8.4 wt% and enables hydrogen desorption at approximately 256 K. The investigation of the dynamic and thermal characteristics of the 8Li-VC system, conducted through ab initio molecular dynamics simulations, provides valuable insights and guidance for future efforts aimed at utilizing this monolayer in hydrogen storage applications with the 8Li-VC arrangement.
Related Concept Videos
Imperfections in Crystal Structure: Stoichiometric Point Defects
Imperfections in Crystal Structure: Non-Stoichiometric Defects